RSS Feeds3-D printing eliminates undesirable trait in conventional superalloys
(PHYSorg.com Chemistry)

 
 

6 december 2018 17:00:10

 
3-D printing eliminates undesirable trait in conventional superalloys
(PHYSorg.com Chemistry)
 


An undesirable trait found in traditionally processed superalloys does not exist in a 3-D-printed, nickel-based superalloy, according to a team of materials scientists who think this could lead to new manufacturing techniques that allow for alloys with tailored properties.


 
13 viewsCategory: Science > Chemistry
 
Researchers find a way to peel slimy biofilms like old stickers
(PHYSorg.com Chemistry)
Chemists find way to prevent side effects from malaria medication
(PHYSorg.com Chemistry)
 
 
blog comments powered by Disqus


Copyright © 2008 - 2024 Indigonet Services B.V.. Contact: Tim Hulsen. Read here our privacy notice.
Other websites of Indigonet Services B.V.: Nieuws Vacatures Science Tweets Nachrichten